Oper Dent ; 27(4): 349-53, 2002.
Artigo em Inglês | MEDLINE | ID: mdl-12120771

RESUMO

This study evaluated the fracture resistance of maxillary premolars with MOD cavity preparation and simulated periodontal ligament. The teeth were restored with silver amalgam (G1), Scotchbond Multi-Purpose Plus and silver amalgam (G2) and Panavia F and silver amalgam (G3). After restorations were made, the specimens were stored at 37 degrees C for 24 hours at 100% humidity and submitted to the compression test in the Universal Testing Machine (Instron). The statistical analysis of the results (ANOVA and Tukey Test) revealed that the fracture resistance of group 2 (G2=105.720 kgF) was superior to those of groups 1 (G1=72.433 kgF) and 3 (G3=80.505 kgF) that did not differ between them.


Assuntos
Dente Pré-Molar/fisiopatologia , Amálgama Dentário/química , Colagem Dentária , Restauração Dentária Permanente/classificação , Fraturas dos Dentes/fisiopatologia , Análise de Variância , Cobre/química , Preparo da Cavidade Dentária/classificação , Análise do Estresse Dentário/instrumentação , Adesivos Dentinários/química , Humanos , Umidade , Maxila , Ligamento Periodontal/fisiopatologia , Cimentos de Resina/química , Prata/química , Estatística como Assunto , Estresse Mecânico , Propriedades de Superfície , Temperatura , Fatores de Tempo
SELEÇÃO DE REFERÊNCIAS
DETALHE DA PESQUISA